MATERIALS & PROCUREMENT
P20 vs H13 Tool Steel for Mold Inserts: What to Specify
Compare the material condition and the complete manufacturing route before comparing two quotations.

P20 and H13 tool steel should be compared through the component’s duty, delivery condition and final treatment requirements. For a mold insert, the material name alone does not define the finished hardness, surface condition or manufacturing route. Start with those requirements before comparing quotations or proposing a substitution.
This guide uses named steelmaker products to illustrate the difference between a prehardened P20-type mold steel and an H13-type through-hardening steel. It supports a specification discussion for custom mold inserts; it does not make the two grades interchangeable.
Key takeaways
- Specify the exact grade, producer and delivery condition when required.
- Separate supplied hardness, final core hardness and any surface treatment.
- Compare machining, treatment, finishing and inspection as one purchasing scope.
- Resolve a proposed material change with the responsible engineer before purchasing or manufacturing.
1. What is the practical difference?
A prehardened mold steel can be machined in its supplied condition when that condition satisfies the design. A through-hardening route introduces a separate heat-treatment decision and subsequent finishing plan. The distinction affects how the buyer defines the order, even before any machining cost is calculated.
For a specific P20-type example, Uddeholm identifies Impax Supreme as a prehardened mold steel supplied at 290–330 HB. Its technical brochure describes it as AISI P20 modified. That range belongs to the named product and condition; it is not a universal delivery requirement for every steel sold as P20.
For a specific H13-type example, Uddeholm lists Orvar Supreme under AISI H13 and describes through-hardening capability, high-temperature strength and resistance to thermal shock and fatigue. The manufacturer also lists use in plastic molds. These characteristics provide a basis for engineering review, not an automatic choice for every cavity insert.
| Specification issue | P20-type example | H13-type example |
|---|---|---|
| Named reference | Uddeholm Impax Supreme, P20 modified. | Uddeholm Orvar Supreme, H13 type. |
| Supplied condition | Hardened and tempered, 290–330 HB. | Soft annealed, approximately 180 HB in the cited brochure. |
| Order decision | Can the specified component use the supplied condition? | What final condition and treatment route does the component require? |
| Finishing question | Which final dimensions and surface requirements remain? | Which features need finishing and inspection after treatment? |
Delivery conditions above are from the Impax Supreme brochure, printed page 3 and Orvar Supreme brochure, printed page 3. Verify the current purchase specification with the supplying steelmaker.
2. Which operating requirements should drive the review?
Describe what the insert must withstand before asking which steel is better. Include the molding material, fillers, operating conditions, contact or sliding interfaces and the reason for any replacement. A worn component, a chipped edge and a corroded cavity do not necessarily call for the same material change.
Uddeholm’s plastic moulding steel guide treats wear, corrosion, toughness and finish demands as material-selection factors. Use those categories to build the brief. Do not select a grade using an assumed shot count or a ranking based only on nominal hardness.
- Wear: identify the affected region and the material contacting it.
- Loading: describe thin sections, supported features, impacts and thermal cycling.
- Surface: state the polish or texture requirement and protected edges.
- Environment: identify corrosion-related conditions and cleaning exposure.
- Replacement: explain whether the drawing is unchanged or an engineering modification is proposed.
If corrosion resistance is a controlling requirement, reopen the grade review instead of assuming that either candidate solves it. If the component works against another insert, include the mating material and relevant fit. A material decision should account for the interface, not only the isolated part.
3. Separate delivery hardness from final hardness
Write the hardness requirement together with its condition and test basis. Supplied-stock hardness, finished core hardness and surface-layer hardness are separate requirements. A hard surface does not establish the properties of the underlying section, and a stock certificate does not show the final condition after later processing.
The Impax Supreme brochure describes use in the supplied hardened and tempered condition and discusses additional treatments for specific requirements. Consequently, “prehardened” should not be read as permission to ignore every later thermal or surface operation.
For an H13-type component, define the required finished condition and have the treatment route reviewed for the exact grade and section. Avoid writing a generic furnace program into the purchasing note. The steelmaker’s guidance, part geometry and heat-treatment provider’s process need to be considered together.
Do not silently convert a manufacturer’s HB delivery range into a customer’s HRC acceptance range. If a different scale or test location is required, agree it explicitly. Keep a measured result distinct from a nominal target or a handbook conversion.
4. Compare the complete manufacturing route
A quotation should identify the material condition at each important handoff. Review rough machining, heat treatment where required, final machining, EDM, grinding, polishing and any surface treatment. Mark which dimensions are accepted only after the final relevant operation.
Orvar Supreme’s technical brochure includes dimensional-change information from defined heat-treatment samples. Those sample results demonstrate why treatment and finishing must be coordinated; they do not establish a universal machining allowance for a customer insert. Agree stock and finishing access for the actual geometry.
For a critical insert, ask which references remain available after treatment and which surfaces will be finished last. A route may be unable to correct a feature if the required tool or measuring probe cannot reach it. Resolve that access problem before ordering the material.
A quotation comparison to avoid
Quote A includes a prehardened material, final machining and inspection. Quote B lists soft-annealed stock and machining but leaves heat treatment and final finishing unspecified. Comparing only the quoted totals does not establish which complete component costs less.
This is a purchasing example, not a customer case. Ask both suppliers to quote the same approved final specification and identify any exclusions.
5. Which records should be agreed before placing the order?
Request the evidence needed to connect the order to the delivered part. Identify material documentation, treatment records and final inspection separately. Confirm their availability and scope before order placement, including any documents supplied by external service providers.
| Record | What to confirm |
|---|---|
| Material document | Exact designation, producer where required, batch reference and delivery condition. |
| Treatment record | Part or batch connection, agreed process scope and required results. |
| Hardness result | Test basis, location where specified and the condition tested. |
| Dimensional report | Drawing revision, final condition, critical features and reporting coverage. |
A catalog data sheet describes a product family. A material record identifies a supplied batch. A dimensional report describes measured component features. Keep all three roles clear when reviewing the evidence; none replaces the others.
6. How to prepare the material request for SENLAN
Provide the approved drawing, exact grade and any required brand or source. Add the supply condition, final hardness, treatment scope, finish zones and required documents. Identify open engineering questions separately from requirements already fixed by the drawing.
SENLAN’s Materials & Heat Treatment page states that specialist suppliers perform heat treatment and that SENLAN rechecks hardness and critical dimensions when parts return. It also states that customer-specified materials are not substituted. A P20/H13 comparison therefore supports a discussion with the responsible engineer, not an unapproved material change.
For finishing requirements, connect the request to precision grinding. For the required records, use Manufacturing & Quality as the starting point and agree the component-specific scope.
Bring the material and drawing into one review
Share the specified grade, final condition and critical features. Identify whether the request is for manufacture to an approved specification or for clarification of an unresolved material requirement.